Home / Articles / Fine-wire stripping in Vietnam

Scaling Wire Harness Production in Vietnam: Keeping Fine-Wire Stripping Consistent

Shenzhen Zirong Hengxun Technology Co., Ltd. · ZIRONX | 2026-11-16

1. What actually gets harder when a harness plant grows in Vietnam

Vietnam has spent a decade absorbing wire harness capacity from Japanese, Korean, European and now Chinese Tier-1 suppliers, concentrated in the industrial belts around Bac Ninh, Bac Giang, Hai Phong in the north and Dong Nai, Binh Duong and Ho Chi Minh City in the south. The pattern is consistent: a plant starts with one or two mature product lines, then volume arrives faster than process maturity does.

Three things break in that gap, and only the first two are usually on the improvement plan:

  1. Equipment capacity — visible, budgeted, solved with a purchase order;
  2. Headcount and training — visible, solved with a recruitment drive and a training matrix;
  3. Process repeatability — invisible until the customer audit, and the one that produces rework, scrap and containment actions.

Fine-wire stripping sits entirely inside the third category.

2. Why fine-wire stripping is the step that does not scale by hiring

Heavier gauges with PVC or PE insulation forgive a lot. The narrow band that does not is high-temperature insulation on fine wire — polyimide (PI / Kapton), PTFE and the PFA / FEP / ETFE family — typically 0.15–1.22 mm, used in aerospace, defence, medical device, sensor and new-energy harnesses.

With a mechanical blade, the outcome is a function of the operator's hand: how deep the blade closed, how hard it was pulled, how long it dwelled. Change the operator and the result changes. On a growing line with high turnover, that means:

  • strip length drifts between shifts, so the crimp nest or the terminal position moves;
  • strand damage appears on a small but persistent percentage of wires, invisible at 1× and fatal in vibration or thermal cycling;
  • rework is discovered downstream, so the cost is paid twice — once to build the wire, once to find and rebuild it.

Thermal stripping removes the hand from the equation: the blade heats the insulation to its softening window and the layer separates with almost no force, so the conductor is never cut. The more useful consequence is procedural — temperature, blade aperture and strip length are all numbers, and numbers can be written into a work instruction and audited.

3. Build an aperture matrix before you buy anything

The most common failure we see is not a wrong machine, it is a missing aperture matrix. Aperture (the hole the blade closes around) must match the wire, and a plant typically runs six to twenty different fine wire sizes.

Blade type Apertures available Use
A type 0.15 / 0.24 / 0.30 / 0.38 / 0.48 / 0.61 mm Fine wires (AWG26–AWG32 range)
B type 0.38 / 0.48 / 0.61 / 0.76 / 0.97 / 1.22 mm Standard range (AWG18–AWG24)
C type Flat blade Very thick or very thin wire, special insulation
D type Custom drilled Non-standard wire sizes

Practical rule: measure the outer diameter of the insulated wire, not the conductor, then choose the nearest aperture. If the aperture is too large, heat transfer drops and the operator raises the temperature to compensate — which is the wrong fix. If it is too small, the wire is crushed before it is heated.

4. Set temperature by insulation family, not by habit

Thermal stripping works inside a softening window, not by burning. Below the window the insulation stays hard and tears; above it the insulation shrinks, discolours, smokes or sticks to the blade, and the conductor is annealed.

The principle to write into the work instruction: find the lowest temperature that separates the insulation cleanly around the full circumference, then set a small margin above it. Relative starting points, to be tuned per supplier and wall thickness:

Insulation Starting point What goes wrong
Polyimide (PI / Kapton) On the high side; tune upward by gauge Thin, tough film: aperture matching matters more than temperature
PTFE High; needs clean blade edges High melt viscosity — will not flow, so it tears if under-heated
FEP / PFA Lower than PTFE Too hot and it strings onto the blade — go low
ETFE Middle band High mechanical strength; between fluoropolymers and ordinary plastics
Silicone rubber Middle-low Elastic — needs support or it stretches instead of separating
PVC / PE Clearly low High heat deforms it, makes it sticky and produces smoke
Enamelled wire Depends on the enamel Very thin film — the parameter window is narrow, always trial first

Change one variable at a time when tuning — 10–20°C steps, three wires per step. Raising by 50°C at a time is how blades get carbonised.

5. Five-point setup checklist for a Vietnam plant

① Power. Vietnam runs 220V / 50Hz. Confirm the input specification before the PO. Equipment that expects 110V, or that needs an external stabiliser, adds a failure mode you do not need.

② Spares. Order a spares kit with the first shipment: at least one spare handle, two blade sets in the most-used apertures, and the power supply or battery pack for portable units. A stopped line waiting for a 300-gram blade is the most expensive kind of downtime.

③ Training. Train on one wire family first, with a written parameter card: aperture, temperature, strip length, dwell. Then extend family by family. Do not train on the full BOM at once.

④ Acceptance criterion. Write down what a good strip looks like: full-circumference separation, no strand damage visible at 10×, strip length within ±0.5 mm, no discolouration of the conductor or plating. This is what an auditor will ask for.

⑤ Documentation. Specification sheet, temperature-verification note, consumable part numbers and recommended stock levels, warranty terms in English. Keep a copy in the plant and a copy in the customer file.

6. The cost model, in three lines

Rework cost per rejected wire = wire + terminal + re-crimp labour + the inspection labour that found it. In most plants that is several times the cost of the strip itself.

If a plant strips 5,000 fine wires a day at a 2% strip-quality reject rate, it rebuilds about 100 wires a day. Multiply by the rework cost and by 300 working days, and compare that number with the invoice price of a stripper. The purchase price is a rounding error; the process is the expense.

This is also the argument a distributor should use with a purchasing manager: not "our blade is cheaper", but "your current rejection rate costs more than the tool".

7. Machine choice by volume

  • Trials, laboratories, mixed low volume: X700 bench-top — 240W constant temperature, 0–700°C with digital blade readout, ESD-safe, alloy + ceramic composite blade.
  • Field, shipboard, on-wing, outdoor installation: B700 cordless — 40,000 mAh, 0–700°C, 3–4 hours at 600°C per charge, 2.5 kg, no mains cable.
  • Volume production with fixed strip lengths: M700 automatic — 100–700°C, strip length 2–40 mm programmable, approximately 3 seconds per wire, AWG18–AWG32.
  • Consumables: T-2 handles and K-700 blades, shared across X700 and B700 — handle stays, blade is replaced.

Sample-wire testing is supported: send the wire specification (gauge, insulation, strip length, daily volume) and we will recommend the model and aperture, strip your sample, and return the result before you commit.

8. For distributors in Vietnam, Thailand and Indonesia

We work through regional distributors rather than direct export sales, with a defined territory, a suggested retail price that protects your margin, a demo-unit policy, spare-parts kits and English technical documentation you can hand to your customers. If you already sell wire processing, crimping or harness equipment, the conversation is short — see the distributor programme.

Sample-wire test / distributor enquiry →